1. … alloy without any risk for cracks and can also be applied on austenitic manganese steels, 300 HB is usually already almost obtained in …
  2. … high temperature creep properties. The weld deposit is fully austenitic and corrosion resistant. … ISO 15608: 8.1  Austenit ≤ 19 % Cr , …
  3. … alloy without any risk for cracks and can also be applied on austenitic manganese steels. The weld deposit is machinable with tungsten …
  4. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat … 6 CrNi 18 9, X 12 CrNi 18 9, G-X 8 CrNi 18 10, X 6 CrNi 18 10, X 10 CrNiTi 18 10,  X 5 CrNi 18 10 AISI 304, 304H, 312, 321H, 347, 347H,  UNS …
  5. … strong, tough Nb-free weld metal for dissimilar welds in Superaustenitic and Superduplex stainless steels or combinations of these with … properties in this situation. … duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, …
  6. … High wear resistance and austenitic structure deposits. The deposit gives already a very good …
  7. … CEWELD® 316H Tig is designed for welding 316/316H austenitic stainless steels operating at high temperatures (500-800°C) under …
  8. … in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone). It is able to withstand a wide range …
  9. … Preheating and interpass temperature 400-450 °C (austenitic welding) or 250-300 °C (martensitic welding). Root passes should …
  10. … A continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. …