1. … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and …
  2. … extreme high strength with excellent ductility and good weldabillity. Preheat and interpass temperature > 200°C …  1.7218, 1.7225 25 CD4, 13 …
  3. … compared to CMn steels and sees the alloy being used for boiler, pressure vessel and piping construction. Typical with FL 155 Flux or FL …
  4. … Can be welded crack free by preheating approxiamately 450°C and keep that also as interpass … for example in an oven. … 56-59 HRc hardfacing alloy, Mixing peddles, Press screws, Kneading machine, screw conveyors, pumps etc. … OA 54 L … …
  5. … as most commercial copper grades. Thicker sections than 5 mm should be preheated up to approximately 500 °C. … Cladding steel, Grey cast iron, …
  6. … of the pure aluminium grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the …
  7. … cobalt-based alloys, allowing multiple layer build-ups with no pre-heating needed. -ULTIMET wire produces deposits wich harden quickly …
  8. … suited for welding jobs at poorly accessible points and badly prepared seams. CEWELD® E 6013 S can be sued in all positions, in …
  9. … type for economic production of creep resistant steels and pressure-hydrogen-resistant 2¼Cr1Mo-steels. Due to the seamless …
  10. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625P …