1. … Use a larger tip than is generally recommended for same diameter mild steel. Use slight excess acetylene feather. The deposit is not … rod or endless on coils. … Dur R (Ni) can be applied on all sorts of steels except on cast iron or Mn-steel. The main applications are hardfacing and rebuilding of …
  2. … for welding fine grained similar alloyed high yield strength steel > 960 MPa in case high impact values are required at sub …
  3. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down …
  4. … grain coarsening. Absence of stabilization means that this steel is distinctly vulnerable to sensitization phenomenon during …
  5. … Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production process the …
  6. … Designed for welding heat resistant steels to sustain working temperatures up to 650˚C … For matching 5%Cr-0.5%Mo creep resisting ferritic steels GX12CrMo5 (1.7362), X12CrMo5 (1.7363), Upto 1180 MPa ASTM: …
  7. … Submerged arc welding wire for fine grain steels where high impact values are required at low temperatures. … …
  8. … Corrosion resistance is higher than 5%Cr-0.5%Mo steels requirements. To be used with shielding gas Ar+O2.   … For matching 9%Cr-1%Mo creep resisting martensitic steels ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 …
  9. … in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling …
  10. … offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to …