1. … Due to the high resistance to cracking and toughness, all weld metal requires no buffer layer. Suited for wear parts subject to heavy … and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening is possible. The maximum hardness is dependent on the base metal and is usualy already achieved in the first layer. … Rails …
  2. … Extremely crack resistant weld metal conditioned by the high basic slag. Low spatter loss, easy slag … for joining high carbon steels and when welding critical mixed base metal combinations. Ideal metallurgical choice for repair welding and production as well as for …
  3. … Due to the high resistance to cracking and excelent toughness, all weld metal requires no buffer layer except on materials considered critical. … and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening is possible. The maximum hardness is dependent on the base metal and is achieved already in the first layer.  … Conveyors and …
  4. … This Nickel - Copper weld metal has properties similar to “Monel 400”. It has good strength and … in many media, including sea water, salts and reducing acids. The weld metal is not age hardenable and when used to join Monel K-500 it has lower strength then the base metal. … 2.4360, 2.4375, NiCu30Fe, NiCu30Al, Monel 400, R405, alloy …
  5. … Due to the high resistance to cracking and toughness, all weld metal requires no buffer layer. Suited for wear parts subject to heavy … and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening is possible. The maximum hardness is dependent on the base metal and is usually already achieved in the first layer. … Rebuilding …
  6. … relieving at 800 °C is recommended if this is permissible for the base metal. In the machined state there should be at least two weld layers on top of each other. The weld metal can be polished and is scale-resistant up to 900°C. The achievable hardness of the weld metal is mainly influenced by the dilution with the respective base …
  7. … Outstanding alloy against high impact combined with abrasion including metal to metal friction and increased working temperatures up to 550 °C. Due to the high resistance to cracking and toughness, all weld metal requires no buffer layer except on materials considered critical. …
  8. Brand: Selectarc
    CEWELD Product: E NiFe 2
    … 52 … Selectarc Bimetal-NiFe …
  9. … blog is your source of information. … EXPLORING THE WORLD OF FILLER METALS AND WELDING TECHNIQUES …
  10. … er een groot aantal nieuwe legeringen ontwikkeld door ons R&D team van metallurgen en er staat nog veel meer op stapel. … VERTROUW OP DE FILLER METAL SPECIALIST …