1. … OA 4370 or OA MnCr is recommended in case of old layers or critical base metals. Equivalent in SMAW: Dur 64 … For fire gratings, sintering …
  2. … Cu-Al-Ni bronze. Sound, pore free deposits on ferrous and non-ferrous base materials. Seawater, wear and corrosion resistance; for example … pressure. Especially suited for marine environments. The addition of nickel improves corrosion resistance in heat and rough seawater. … …
  3. … S 32101. Due to the higher Mn and N – content of the Lean duplex base material, the slag viscosity and therefore the flow behaviour is …
  4. … The deposit is free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling …
  5. … interpass temperature and post weld treatment as required for the base metal. Hydrogen content: HD < 3 ml / 100 g weld metal. CEWELD E …
  6. … 2400 HV Iron and Tungsten based hardfacing alloy containing 52-58% (depending on wire …
  7. … is high-temperature resistant with very good creep resistance. High nickel gives the alloy good resistance to carburisation and under …
  8. … OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … 64-68 HRc Hardfacing wire used in mining, agriculture …
  9. … Sound, pore free deposits on ferrous and non-ferrous base materials. … Cunifer 10, cuni10fe, seawater resistant, marine …
  10. … Like other nickel alloys, it is ductile, easy to form and weld, and possesses … of chlorides and other halides. … Alloy C-2000, 2.4675, Ni99,2, Nickel 200 … Alloy C-2000 … A 5.14: ERNiCrMo-17 … 18274: S Ni …