1. … staan garant voor zeer stabiele mechanische waarden zelfs na langdurig gloeien. Deze elektrode is bovendien door DNV gekeurd in de …
  2. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  3. … Welding procedure (including preheat temperature, interpass temperature and PWHT) …
  4. … up to much higher temperatures. Preheating is recommended at 150 - 350° C. depending on the thickness of the base metal. Similar base …
  5. … The filler metal shows remarkable bonding properties and fluididity during welding. … AL 2219, AL 2014; AlCu-cast-alloys, not suitable for …
  6. … Good resistance against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately …
  7. … alloy containing Nickel for more strength and bridging capability during brazing. Due to the special flux coating this type is mostly …
  8. … third parties that enables you to use only one wire to cover more procedures up to 460 MPa yield strength steels. CEWELD AA M460 can also be … Gr. A, B, C; A 181 Gr. 60, 70; A 283 Gr. A, C; A 285 Gr. A, B, C; A 350 Gr. LF1; A 414 Gr. A, B, C, D, E, F, G; A 501 Gr. B; A 513 Gr. …
  9. … resistance to intercrystalline corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon …
  10. … of old layers or critical base metals.. Equivalent in SMAW: CEWELD® Dur 62S  … Trash crushing, impact resistant   … OA 50 … 14700: T Fe16 …