1. … a long life for several wear applications. Best to be used with shielding gas M13 (Argon with 1% Oxygen) approx. 15 litres per minute. … Rebuilding of stabilisers and other oilfield tools where maximum protection … decanter screws or hardfacing deep drilling equipment. … OA WC2 Ni … 14700: T Ni20 …
  2. … Suitable for downhand butt- and fillet weld, smooth welding pool without spatter loss, easy slag release, very nice bead …
  3. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and age Hardfacing components where heat …
  4. … Without slag. Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production …
  5. … above 815 °C (1500°F) up to 1149 °C (2100°F), especially when welding on base metals of nickel-iron-chromium alloys. … Inconel alloys …
  6. … impact values makes this electrode a excellent choice for critical welding applications.  … Screening steels Tools steels* Low alloyed steels … 45C4*, manganese steels, X120Mn12, 1.3401, C45, dissimilar joint welding between steel and stainless steel such as: Armor plate, high carbon steels. Recommended for welding rails, crossing, crusher teeth, hammers and applications where …
  7. … and oxidation resistance above 1150 °C ( 2100 °F), especially when welding on base metals of nickel-iron-chromium alloys. High mechanical …
  8. … hot cracking resistance and mechanical properties. To be used with welding flux FL 8111 or FL 838 … 1.4507, 1.4410, 1.4468, 1.4515, 1.4517, …
  9. … Outstanding hardfacing alloy against abrasion and corrosion combined with high temperatures. … Stellite 1 alloy for cladding, … DUR 1 Tig … A 5.21: ERCoCr-C … 14700: S Co3 …
  10. … production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium alloys with maximum 4% Nickel … Al 4Ni0,2Ti Tig …