1. … against heavy abrasion. Usualy the maximum number of layers is 2 till 3 but when using a special stringer build up technick with release …
  2. CEWELD® AA R690 was one of “The first seamless rutile FCW with extreme low hydrogen for S690” Excellent for use in positional welding where high deposition rate is required, suitable for temperatures down to -60 ºC ( with offshore Approval down to -40°C). Excellent for use on ceramic backing and …
  3. … MPa. Under the different trade names there are many confusions, sometimes standard brass is called Manganese bronze and there are also …
  4. … deposit is capable of taking a high polish.Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / E347, 19 9 …
  5. … resistance to galling. It has cavitation-erosion resistance ten times that of 304 stainless steel, DUR 6 can be used to protect bearing …
  6. … the lowest schrinkage possible to avoid cracks during heating and the cooling period. The weld deposit also retains good strength and …
  7. … will remain very well at increased temperatures. Scale resistant till 900°C.CEWELD MA 617 is best to be used with Ar/Co2 - 98-2.  … …
  8. … better elevated temperature properties than Grade 2 or 3 and is sometimes specified for pressure vessels or piping for its superior …
  9. … the weld and provides protection. Helium or argon/helium mixtures sometimes are used for torch shielding if added penetration is desired. …
  10. …                           3 Layer: 61 - 65 HRc For the best results 2 till 3 layers should be welded. … Sugar mill knives and Hammers, Cement …