  • PRODUCT SPECIFICATIONS
  • PACKAGING
Type
Basic Ni alloyed low hydrogen electrode for stick welding
classification
AWS
A 5.5: E 8018-C2
EN ISO
2560-A: E 46 6 3Ni B 3 2 H5
Applications

Recommended for fine-grained steels used at low temperature (-60 to -80ºC ).Cryogenic and petrochemical industries. Stocking and distribution of liquid gas or products volatile.

Type
Basic Ni alloyed low hydrogen electrode for stick welding
Applications

Recommended for fine-grained steels used at low temperature (-60 to -80ºC ).Cryogenic and petrochemical industries. Stocking and distribution of liquid gas or products volatile.

Properties

Basic, Nickel alloyed (above 3%) electrode with excellent welding characteristics and easy slag removal. Extreme tough welding deposit with guaranteed excelent mechanical properties at low temperatures.HD < 5 ml/100

Classification
AWS
A 5.5: E 8018-C2
EN ISO
2560-A: E 46 6 3Ni B 3 2 H5
F-nr
4
FM
1
Suitable for

Reh ≤ 460 MPa ISO 15608: 1.2, 1.3, 2.1, 9.2 

1.5637, 1.6217, 1.6228, 1.0044-1.0982

10Ni14, 12Ni14, 13MnNi6-3, 15NiMn6, S275N-S460N, S275NL-S460NL, S275M-S460M, S275ML-S460ML, P275NL1-P460NL1, P275NL2-P460NL2 

ASTM A 203 Gr. D, E; A 333 Gr. 3; A334 Gr. 3; A 350 Gr. LF1, LF2, LF3; A 420 Gr. WPL3, WPL6; A 516 Gr. 60, 65; AA 529 Gr. 50; A 572 Gr. 42, 65; A 633 Gr. A, D, E; A 662 Gr. A, B, C; A 707 Gr. L1, L2, L3; A 738 Gr. A; A 841 A, B, C 

NFA 35-207: A510PP1 – A550PP2

NFA 36208: 3.5 Ni 285 ct 355 (12N14)

 

 

Welding positions
PA
PB
PC
PD
PE
PF
Redrying
350°C / 2 hr
Analysis
C Si Mn P S Cr Ni Mo V Cu Nb N Al
0.15 0.3 0.9 0.02 0.02 3.5
Mechanical Properties
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Impact Energy (J) ISO-V Hardness
-80°C -100°C
As Welded 500 620 21 75 30 HRc
e-8018-c2-stick-welding-electrode-for-3-nickel-steels
e-8018-c2-stick-welding-electrode-for-3-nickel-steels
Packing info
E 8018-C2 2,5 x 350mm
Packaging KG/unit EanCode
Can 8720663401335
E 8018-C2 3,2 x 350mm
Packaging KG/unit EanCode
Can 8720663401359