1. … constructions that needs post weld heat treatment after welding and still offers excellent impact properties. … P235GH, P265GH, P295GH, …
  2. … as your IP address, browser type, the pages you have visited, and the times of your visits.   2. Use of Information We use the collected …
  3. … deposit is capable of taking a high polish. Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / E347, 19 9 …
  4. … deposit is capable of taking a high polish.Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / E347, 19 9 …
  5. … the lowest schrinkage possible to avoid cracks during heating and the cooling period. The weld deposit also retains good strength and …
  6. … resistance to galling. It has cavitation-erosion resistance ten times that of 304 stainless steel, DUR12 can be used to protect bearing …
  7. … will remain very well at increased temperatures. Scale resistant till 900°C.CEWELD MA 617 is best to be used with Ar/Co2 - 98-2.  … …
  8. … the weld and provides protection. Helium or argon/helium mixtures sometimes are used for torch shielding if added penetration is desired. …
  9. … offering satisfying results although the old method (pressing twice) still offers the best weldability, but a special press is needed and …
  10. … with very low hydrogen content. Suitable for heat treatment. Step cooling is possible. High reserve of toughness and crack resistance. …