1. … product- of bedrijfspresentaties en biedt plaats aan maximaal 100 personen. De indeling van de zaal kan worden aangepast aan uw …
  2. … The electrode has a soft but intensive welding character, a fine-structured …
  3. … strength and oxidation resistance above 816°C (1500°) up to 1149°F (2100°F), especially when welding on base metals of nickel-iron-chromium …
  4. … to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage in unconditioned condition. … …
  5. … to the seamless production process the hydrogen content is below 3ml/100g weld metal even after long storage in unconditioned conditiond. …
  6. … to the seamless production process the hydrogen content is below 3ml/100g weld metal even after long storage in unconditioned condition. … …
  7. … High C-, Cr-, B-alloyed flux-cored wire electrode which forms extremely hard carbides for extremely hard …
  8. … material or old hard facing layers it is necessary to buffer with an electrode like CEWELD E DUR 350 Kb / E 11018-G that delivers a welding …
  9. … input should be kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high …
  10. … low spatter loss, easy slag removal and hydrogen content below 3 ml/100g. even after long unconditioned storage. … ReH ≤ 460 MPa (67 ksi) …