1. … Special alloyed copper wire for Mig and Tig welding.       The weld metal is a Cu-Al bronze with high aluminium …
  2. … required as alloys of such chemistry are sensitive to embrittlement at 600-800 °C. The interpass temperature should not exceed 300 °C. … … G-X40CrNiSi 27 4, AISI 327, 442, 446, ASTM A 297 HC UNS S44200, 44600, J92605, J93005, J92605  … 4820 AC … 3581-A: E 25 4 R 32 …
  3. … oxidation, at service temperatures ranging from 1200°F (650°C) up to 1600°F (870°C) … AMS 5708, 5709, 5706, 5707, 5704, 5544, 5586. PWA 1005, …
  4. Brand: Selectarc
    CEWELD Product: ER 80S-B2
    … Existe en TIG … 52 … SELECTARC F63 …
  5. … est une électrode sous-marine avec un enrobage de base combiné à une tige centrale à très faible teneur en carbone. AquaForce HR est une …
  6. … • High quality alloyed copper wire for the Tig process (Mig brazing as well) • The weld metal is a Copper- Silicon …
  7. Brand: Selectarc
    CEWELD Product: ER 100 S-G
    … Existe en TIG … 52 … SELECTARC F77 …
  8. … cleaner and higher quality welds, especially when used for the Hotwire Tig process intermediate cleaning between the layers can be skipped and … - NiCr21Mo - 8XNi9 ASTM: A 533 Gr1 UNS: S31254 - N08800 - N08810 - N06600 - N06625 - N08825 - N08926 - N08020 Alloy 254 SMO - Alloy 800 - Alloy 800H - Alloy 600 - Alloy 625 - Alloy 825 - Sanicro 28 … NiCro 625 … A 5.14: …
  9. … 308H and 316H, operates in temperatures up to 800 °C. CEWELD® 16.8.2 Tig gives a very high resistance to thermal embrittlement. Creep …
  10. … abrasion resistance can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For …