- … copper-aluminum alloy without Zn with high toughness and improved hardness. “Very good weldability compare to the more common Al. …
- … even at higher temperatures. The deposit gives already a High hardness in the first layer. A buffer layer is recommended in case of … protective gas.Corresponding electrode: CEWELD® Dur 62 S … 61-64 HRc hardfacing alloy, Cement, Mineral mixing, hammers, coke wear plates …
- … buffer layer except on materials considered critical or in case of old hardsurfacing layers. The weld deposit can be aplied completely crack …
- … abrasion combined with impact. The deposit gives already a very good hardness in the first layer. The choice for the buffer layer is depending on the base metal and not always necessary. … 55-57 HRc hardfacing alloy against shocks and mineral wear, rollers and crushers, …
- … comparable or surpassing Waspaloy and approaching R-41 and Alloy 263 hardenable High temperature dynamic applications … HAYNES® 282® alloy, …
- … for the repair of the capillary losses of brazed joints with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding …
- … sea water, salts and reducing acids. The weld metal is not age hardenable and when used to join Monel K-500 it has lower strength then …
- … and corrosion at high working temperatures upto 900°C. Crack free hard facing deposit against severe shock and impact. … CoCr-E Co1 …
- … of tungsten carbides embedded in a steel matrix. The extraordinary hardness of the fused tungsten carbides (WSC) of approx. 2300 HV imply …
- … Outstanding hardfacing alloy against abrasion and corrosion combined with high …