1. … critical because of its low operating temperature.  Flux/Paste: CEWELD Super-Flux … Copper to Copper (without flux). Brass, Copper and …
  2. … important steps to prevent hydrogen induced cracking are: 1)  Use airtight packing for covered electrodes 2)  Use seamless fluxcored wires …
  3. … solidification and reheat cracking. NILO Alloy 36 is available for Tig, Mig and SAW process. … NILO Alloy 36, Invar, cast Iron … NILO …
  4. … for handling of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material …
  5. … cleaner and higher quality welds, especially when used for the Hotwire Tig process intermediate cleaning between the layers can be skipped and …
  6. … Nickel Iron based filler metal for joint welding and claddings on cast Iron. Very wel …
  7. … wire offers a unique welding deposit with less than 1% nickel to full fill NACE requirements and cover more procedures up to 500 MPa yield …
  8. Brand: Selectarc
    CEWELD Product: ER 80S-D2
    … Existe en TIG … 52 … SELECTARC F60 …
  9. … resistance is comparable to that for other gamma-prime-strengthened superalloys. CEWELD® Alloy 263 is an age-hardenable …
  10. … wire for offshore requirements upto S460 steels that have to fullfill impact requirements down to -60 degrees Celsius and parts that …