1. … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …
  2. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall …
  3. … responsible for its creep strenghth are kept above the minimum considered necessary to ensure satifactory performance. … For matching P91, …
  4. … L-Ag27 is a Very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C (without …
  5. … all weld metal requires no buffer layer except on materials considered critical or in case of old hardsurfacing layers. The weld deposit …
  6. … Abkühlzeit: Die Abkühlzeit zwischen 800°C und 500°C t8/5 ist der wichtigste Parameter, um die Schweißparameter beim Schweißen von …
  7. … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …
  8. … down position with high speed and deep penetration. Due to the wood powder based coating the weld puddle is super fast freezing and therefore …
  9. … Solid welding wire with excellent welding properties under mixed gas M21 (pure Argon for the Tig process) suitable for high …
  10. … rare-earth additions for increased oxidation resistance, especially under conditions of frequent switching or wide temperature fluctuations. …