1. … between 1020°C (1875°F) and 1050°C (1925°F) for one hour, followed by precipitation hardening between 612°C (1135°F) … Suitable for precipitation hardening stainless steel used for welding materials of …
  2. … 10 KJ/cm. Cooling time (T8/5) must be adjusted by travel speed and preheat temperature. … S890 TM-pipe steels to StE 890 to S890QL1, A …
  3. … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg3, AlMg4, …
  4. … metal requires no buffer layer. Suited for wear parts subject to heavy pressure, impact and shock. The interpass temperature should be maximum …
  5. … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000 … Alloy C-2000 …
  6. … used on the back surface of sheet or plate less than 1/4 in. thick to prevent oxidation. Gas Requirements. Welding-grade argon (99.999 …
  7. … Welding procedure (including preheat temperature, interpass temperature and PWHT) will be dependent … kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high …
  8. … 4.2-5.5 g/cm³ (dependent on designated size) Particle shape: preponderantly spherical Typical grain size for sale: -53+22 μm ask for …
  9. … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000, 2.4675, …
  10. … Can be welded crack free by preheating approxiamately 450°C and keep that also as interpass … for example in an oven. … 56-59 HRc hardfacing alloy, Mixing peddles, Press screws, Kneading machine, screw conveyors, pumps etc. … OA 54 L … …