1. … even at higher temperatures. The deposit gives already a High hardness in the first layer. A buffer layer is recommended in case of … material or old layers. Weldable without protective gas … 63-67 HRc hardfacing alloy ,Fan blades, Bucket lips, Mining, Cement, Mineral hammers, coke wear plates etc. … OA 63 … 14700: T Fe15 …
  2. … and the electrodes can be bent very well to improve accessibility to hard to reach places.  … Rp< 380 MPa (52 ksi) ISO 15608: 1.1,1.2, (1.3) …
  3. … SA 420C offers fair general corrosion resistance combined with high hardness and excellent wear properties especially to face metal to …
  4. … Austenitic deposit with strain hardening properties and no limmits in the number of layers. The …
  5. … This nickel based alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. …
  6. … be kept low (as for Mn steel). The weld deposit is offers strain hardening properties from 250 till 450 HB … austenitic manganese steel, high impact loads, hammers, crushers, rebuilding, hardfacing, rails, crossings, Breaker teeth, etc.. … E DUR Mn14 … A …
  7. … thickness due to a high amount of Borium carbides. A extreme high hardness is already achieved in the first layer. The weld deposit will … conveyor chains, agriculture, construction, mixer blades, paddles, cement pumps, screw conveyers, sintering lines, earth moving equipment …
  8. … sophistiqués qui nous permettent de travailler rapidement et efficacement au traitement de vos commandes. La qualité, la fiabilité de la …
  9. … This nickel based alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. …
  10. … to 550°C. as for similarly alloyed steels, quenched and tempered for cementation and nitrating. Hydrogen content: HD < 5 ml/100 g weld metal …