- … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …
- … at very low currents. It is easy to use and inexperienced welders will have no difficulties to produce smooth deposits mainly …
- … sea water, salts and reducing acids. The weld metal is not age hardenable and when used to join Monel K-500 it has lower strength then …
- … stainless steels operating at high temperatures (500-800°C) under long term creep conditions. This filler metal can also be used for …
- … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall …
- … High nickel gives the alloy good resistance to carburisation and under oxidising conditions high chromium provides useful resistance to …
- … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
- … where improved corrosion resistance in specific media is needed. In order to reduce the propensity for fissuring and hot cracking, the low …
- … It produces dense, wellbonded coatings with excellent machineability. … …
- … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …