- … wires. Excellent weld metal quality and X-ray soundness. Post weld heat treatment (PWHT) can be applied without any problems. … 19% Cr / …
- … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA …
- … with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low operating temperature. …
- … hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900°C. DUR 12 offers a low coefficient of friction …
- … deposit is capable of taking a high polish.Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / E347, 19 9 …
- … and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg3, AlMg4, …
- … a full high hardness in the total thickness of the plate. No excessive heat that effects the basemetal or cause loose in strength two times …
- … welding properties. Stainless deposit with low carbon content. Low heat input is recommended to avoid pronounced grain coarsening. Absence …
- … of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 (1.4718) …
- … hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900°C. Dur 12 offers a low coefficient of friction …