1. … CEWELD® ER 80S-B3L Tig is a low alloy copper-coated TIG rod with 2.25% Cr and 1% Mo content, with low carbon content (less … 10H2M, B.S. grade 45, K21390, K21590, J22091, J21890 … ER 80S-B3L Tig … A 5.28: ER80S-B3L … 21952-B: W 2C1ML …
  2. AlSi12 was originally developed as a brazing alloy to take advantage of … freezing range. In addition, it has a higher silicon content than AlSi5, which provides increased fluidity and reduced shrinkage. Hot cracking is significantly reduced when using AlSi12 as a filler alloy. The alloy may be used in applications at …
  3. CEWELD Product: AlSi 5
    … 274 … RE-ON TIG AlSi 5 …
  4. … sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, AlMg1SiCu, 3.3206, 3.3210, 3.2315, 3.3211, EN AW 6060, EN AW 6005A, EN AW 6082, EN AW 6061, EN AC 45000, … AlSi 5 Tig … A 5.10: ER4043 … 18273: S Al 4043A (AlSi5(A)) …
  5. CEWELD Product: AlSi 12
    … 274 … RE-ON TIG AlSi 12 …
  6. … CEWELD® AlSi12 Tig was originally developed as a brazing alloy to take advantage of … freezing range. In addition, it has a higher silicon content than AlSi5, which provides increased fluidity and reduced shrinkage. Hot … 3.2151, B 413.0, 361.0, 359.0, 356.0, 319.0, Cast aluminium … AlSi 12 Tig … A 5.10: ER4047A … 18273: S Al 4047A (AlSi12(A)) …