1. … hand welding. Excellent against pitting and stress corrosion. The PREN above 35 weldmetal offers outstanding resistance against pitting. …
  2. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  3. … free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you …
  4. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  5. … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected …
  6. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  7. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or …
  8. … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO …
  9. … CEWELD® SA 318 is engineered to a very precise analysis to create a weld deposit of high purity, superior hot …
  10. … and down hand welding. Excellent against pitting and stress corrosion.PREN above 35 weldmetal offers outstanding resistance against pitting. …