1. … where improved corrosion resistance in specific media is needed. In order to reduce he propensity for fissuring and hot cracking, the low …
  2. … weld metal composition of 12% Chromium. These weld deposits are air-hardenable that can normally be heat-treated after welding. … 1.4000, …
  3. … Austenitic deposit with strain hardening properties and no limmits in the number of layers. The deposit …
  4. … Alloy C276 is a popular nickel-molybdenum-chromium alloy renowned for its exceptional corrosion resistance …
  5. … offers a easily machinable weld deposit with high ductility and no undercut. … Welding ductile, grey and malleable cast irons. Ni 99 can …
  6. … and joining of Copper and CuSn-Alloys. Widely used in oven soldering. High quality alloyed copper wire. Sound, pore free deposits and … and joining of Copper and CuSn-alloys. Widely used in oven soldering. Mat.n: 2.1010, 2.1016, 2.1020, 2.1030, 2.1050, 2.1052, 2.1056, …
  7. … and 1050°C (1925°F) for one hour, followed by precipitation hardening between 612°C (1135°F) … Suitable for precipitation hardening stainless steel used for welding materials of similar chemical …
  8. … All our seamless fluxcored welding wires undergo a full 3.1 all weld metal test according EN 1597. In addition …
  9. … snel mogelijk reageren! kijk in je mailbox voor de bevestiging. We waarderen je interesse in onze producten en service.  Een hele fijne dag …
  10. … optimum deposit rate and metallurgical quality and attractive welder appeal in the PA-PB position. Very good resistance against pitting …