1. … metal has low levels of tramp elements (eg. Sn, As, Sb and P) providing a low Bruscato Factor.(X …
  2. … Rutile stick electrode for welding of steam production plants, steam pipes and similar joints made of … quenched and tempered for cementation and nitrating. … Typ 1Cr 0,5Mo, ISO 15608: ~5,1 1.7335, 1.7262, 1.7728, 1.7218, …
  3. … for use of short arc and spray arc. Excellent gap bridging for root welding. High-efficiency type for economic production enviroments and … long storage in unconditioned condition. … Typ 0,5Mo  ≤ 460 MPa,  ISO 15608: 1.2, 1.3 1.5415, 1.0481, 1.0482 15 Mo3, 16Mo3 , 20MnMoNi4-5, …
  4. … of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, AlMg5, AlMg2Mn0,8, AlZnMg1, …
  5. … basic SAW flux with low hydrogen content. Basicity: About 3,4 (according to Boniszewski) Current: DC or AC, in single or multi-wires Grain …
  6. … should be between 100°C (212 °F) and 150°C (302 °F) . As welding flux FL 155 should be used because of its high basicity and low hydrogen content. … Reh < 890 Mpa Iso 15608: 3.2 (Reh > 690 MPa) 1.8796, 1. 8925, 1.8940, 1.8983, 1.8797, …
  7. … The  alloy deposit can be machined  with tungsten tool tips and by grinding. The hardness of the deposit will degrease 16% at 300°C and about …
  8. … or toughness. Grade 5 is used in aircraft components such as landing gear, wing spars, and compressor blades. Its corrosion resistance …
  9. … Extreme easy to weld with excellent welding properties. High world wide excepted quality with controlled cast … offers excelent weather resistant properties.  … CuNi, Reh ≤ 460MPa ISo 15608: 1.4 1.8963, 1.8946, 1.8965 S235JRG2Cu, S235J2G4Cu, S235J0Cu, …
  10. … The CEWELD® 904L is used for welding materials of similar chemical composition which are used for …