1. … down to -60 °C. Excellent welding properties.  Yield strength < 600 MPa. Low hydrogen content  HD< 3 ml/100g even after long storage. … …
  2. Brand: Böhler Welding
    CEWELD Product: AA NiCro 600
    … FOXcore Nicro 83-T0 … 235 … NIBAS 70/20 Mn-FD …
  3. … and by grinding. The hardness of the weld deposit will degrees 20% at 600 °C and has a nominal hardness of 49-53 HRc at room temperature. The …
  4. … and by grinding. The hardness of the weld deposit will degreas 20% at 600°C and has a nominal hardness of 47-52 HRc at room temperature. The …
  5. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  6. … 279°C / Deposit color: Silver / Shear Strength (copper lap joint): 10,600 PSI … Copper, stainless steel … S-SnAg5 …
  7. … required as alloys of such chemistry are sensitive to embrittlement at 600-800 °C. The interpass temperature should not exceed 300 °C. … … G-X40CrNiSi 27 4, AISI 327, 442, 446, ASTM A 297 HC UNS S44200, 44600, J92605, J93005, J92605  … 4820 AC … 3581-A: E 25 4 R 32 …
  8. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel … Alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X … A 5.14: ERNiCrMo-2 … 18274: S Ni 6002(NiCr21Fe18Mo9) …
  9. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°C) for 16,000 hours. Suitable for joining and … alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X Tig … A 5.14: ERNiCrMo-2 … 18274: S Ni …