- … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable with carbide tip tools, hardening …
- … be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or …
- Brand: Selectarc52 … SELECTARC D25/09 …
- Brand: SelectarcCEWELD Product: 2594 Super Duplex52 … SELECTARC D25/09W …
- Brand: SelectarcCEWELD Product: AA 2594… 52 … SELECTARC FCW 2509MO …
- Brand: AvestaCEWELD Product: SACW 2594 Super Duplex… 36 … 2507/P100 …
- CEWELD Product: E DUR 300 Kb… 275 … HARDMELT 250 …
- CEWELD Product: SG CrMo1… 45 … Lastek 250C …
- Brand: Lincoln ElectricCEWELD Product: E NiCrMo 686 CPT… 46 … Jungo SD 2509 …
- Brand: Böhler WeldingCEWELD Product: 2594 Super Duplex235 … Böhler Thermanit 25/09 CuT …