1. … and hydrogen content below 3 ml/100gr. even after long unconditioned storage. … CuNi, Reh ≤ 460MPa ISo 15608: 1.4 1.8963, 1.8946, 1.8965 …
  2. … zones of welded joints. Resistance to general, pitting and crevice corrosion increases with the alloying (Cr+Mo+W) content, and …
  3. … the hydrogen content is below 3ml/100g weld metal even after long storage in unconditioned condition. Good gap bridging properties. … Typ …
  4. … excellent resistance to stress & corrosion cracking, pitting and crevice corrosion. High mechanical properties with excellent weldability … wetting compare to solid wire. Aggresive media, against pitting and crevice corrosion, dissimilar joint of nickel alloys and stainless …
  5. … intermediate strength grade originally developed to provide enhanced crevice-corrosion resistance in high temperature brines, but at lower … ions that alter the surface electrochemistry of the material in the crevice or under a surface deposit. Grade 12 has better elevated …