1. … plasticity of the weld deposit. Weldable with Co2 and Mix gas. … Reh ≤ 960 MPa ISO 15608: ~3.1, 3.2 (Reh > 690 MPa) 1.8796, 1. …
  2. … denn je ist das Erstellen bzw. Überholen von Versorgungspipeline für Gas/Wasser u. andere Medien. Hier bieten wir mit unserem neu …
  3. … content also confers resistance to high-temperature corrosion in gases having an oxidising and sulphidising effect. Due to its high …
  4. … subject to excessively heavy abrasive wear weldable without protective gas. Extreme good wear resistance even at higher temperatures up to …
  5. … up to ~600°C particularly in environments involving hot hydrogen gas. Flux CEWELD® FL 880 … ASTM: A 182 Gr F9, A 199 Gr T9 , A 213 Gr T9 …
  6. … subject to excessively heavy abrasive wear weldable without protective gas. More than 3 layers should not be deposited. A Buffer layer with OA …
  7. … temperatures down to -60 °C. Applications include structural, oil and gas and offshore steelwork. … Reh ≤ 960 MPa ISO 15608: ~3.1, 3.2 (Reh > …
  8. … scale-resistant up to approx. 800°C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish.Structure: …
  9. … a long life for several wear applications. Best to be used without gas protection (self shielded). … Rebuilding of stabilisers and other …
  10. … up to approx. 800 °C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish. … ISO …