1. … should be between 100°C (212 °F) and 150°C (302 °F) . As welding flux FL 155 should be used because of its high basicity and low …
  2. … flux FL 880 excellent results are obtained for both joining and cladding applications with self lifting slag and it leaves a fine rippled …
  3. … silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low operating temperature.  Flux/Paste: …
  4. … Rutile stick electrode for welding of steam production plants, steam pipes and similar joints made of …
  5. … to the Titanium carbides. The choice for the buffer layer is depending on the base metal and not always necessary.  … HRc 54-59, … gravel pumps, bucket collars, dredger teeth etc. … OA 55 TC … 14700: T Fe8 …
  6. … Excellent welding properties with high build-up capacity and low dilution rate. … medias. Excellent fatigue strength and creep properties. … Cladding against high temperature, radiant heater tubes, furnace rolls, …
  7. … Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with yield strength > 690 MPa. Crack resistant …
  8. … and oxidation resistance up to about 800 °C. Excellent rolling and sliding properties in metal-to-metal wear applications, among others. … … running surfaces of heavily loaded PTO shafts, etc. … E DUR 600 Kb … 14700: E Fe8 …
  9. … at sub zero temperatures down to - 60 °C (-80°C). Excellent welding properties. Therefore, suitable for the economic processing of …
  10. … impact and pressure loads applications. Best to be used with welding flux FL 915 … Rebuilding rails, crossings, crushing hammers, dredger teeth, rollers, blast … Hardfacing manganese hard stee, buffer layers etc.. … SACW MnCr … 14700: T Fe9 …