1. … Basic electrode for welding of steam production plants, steam pipes and similar joints made …
  2. … Submerged arc welding (5% chromium wire) for high temperature creep resistant steels. …
  3. … deposits are air-hardenable that can normally be heat-treated after welding. … 1.4000, 1.4001, 1.4002, 1.4003, 1.4006, 1.4008,  1.4021, …
  4. … production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium alloys with maximum 4% Nickel … Al 4Ni0,2Ti Tig …
  5. … mechanical properties. Due to the addition of Sn. this alloy will show a bright looking joint and is more capillary then the standard …
  6. … against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately the composition …
  7. … excellent wetting. Due to the excellent wetting and low melting point welding speeds can be achieved upto 2 mtr/min. The weld deposit offers …
  8. … The electrode is an exceptionally versatile product for dissimilar welding. It can be used on a variety of austenitic and ferritic steels …
  9. … rutile flux with Mn and Si pick-up, suitable for carbon steel welding with two or three passes. Basicity: about 1,7 (according to …
  10. … Hardfacing layers should be removed, clean or grind properly before welding. … Gear parts, recycling wear blocks, cutters, molds, pumps, …