1. … resistant to stress corrosion cracking which can occur in the primary water loops of nuclear power stations. The material also shows …
  2. … grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of being …
  3. … a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and (semi)automatic …
  4. … in aqueous solutions and can be operated up to maximum 650°C (1202°F). Primary WC carbide size: 2.5 μm FSSS Apparent density (ISO 3923-2) …
  5. … Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, AlMg1SiCu, …
  6. … Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11 G-AlSi12 (Cu), G-AlSi7Mg, …
  7. … during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding Aluminium alloys with …
  8. … Users are cautioned to confirm by qualification testing, or other appropriate means, the suitability of any welding consumable and procedure …
  9. … Welding-grade argon (99.999 percent purity) usually is chosen for primary, secondary, and backup shielding, as well as for purging. Argon …
  10. … en traceerbaarheid van uw goederen is onze hoogste prioriteit.  Alle productcertificaten volgens EN 10204 zijn 24 uur per …