1. … de enige rutiel gevulde draad ter wereld in deze klasse (T 62 4) SMAW: Ceweld 10018-D2 , hier gaat het om een volledig nieuw ontwikkelde …
  2. … The weld puddle is amazingly fast freezing and therefore especially preferred in vertical down position with high speed and deep …
  3. … one of “The first seamless rutile FCW with extreme low hydrogen for S690” Excellent for use in positional welding where high deposition … 1.8927, 1.8931, 1.8928, 1.8974,  1.7147, 1.7149, 1.8734 S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, 20MnCr65, 28CrMn4-3 L480 - L550, X65, … Q, 620 QL, 620 QL1, aldur 700 Q, 700 QL, 700 QL1, Salzgitter S700MC, Ympress Steel E690 TM, S700MC, Amstrong Ultra 650MC, 650 MCt, 700 MC….. … …
  4. … The presence of tin improves the fluidity and is useful to increase the …
  5. … cobalt-based alloys, allowing multiple layer build-ups with no pre-heating needed. -ULTIMET wire produces deposits wich harden quickly …
  6. … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  7. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  8. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625 …
  9. … Can be welded crack free by preheating approxiamately 450°C and keep that also as interpass … for example in an oven. … 56-59 HRc hardfacing alloy, Mixing peddles, Press screws, Kneading machine, screw conveyors, pumps etc. … OA 54 L … …
  10. … and well suited for low-temperatures, ductility down to -60°C. Preheating, interpass temperature and post weld treatment as required … 1.8914, 1.8927, 1.8931, 1.8928, 1.7147, 1.7149, 1.8734 S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, 20MnCr65, 28CrMn4-3 L480 - L550, X65, X80, …