1. … properties as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/hour to 620ºC than Air Cool for 8 hours … Inconel 718(2.4668), 706 and X-750 (X750) … NiCro 718 Tig … A …
  2. … at 760 °C for three minutes / mm wall thickness at least for 2 hours. Tempering, if specified, at 1050 °C for 1/2 hour/oil and annealing at 760 °C for 2 hours. … 1.4935 X20CrMoWV12-1, 1.4922 X20CrMoV12-1, 1.4923 …