- … to be used in corrosive environments, normally without post-weld heat treatment. At 33% nickel, CEWELD® 320 Tig has practical immunity …
- … higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or AA …
- … cobalt-based alloys, allowing multiple layer build-ups with no pre-heating needed. -ULTIMET wire produces deposits wich harden quickly …
- … L-Ag20 is a Silver-containing, superheat-resistant silver solder alloy without Cadmium for gap and joint … Cast Iron. Also suitable for dissimilar joints between these metals. Heat resistant up to 300°C. … L-Ag20 … 17672: Ag 220 …
- … SA 310 is a corrosion-resistant, chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. He has …
- … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA 310B …
- … deposit is capable of taking a high polish. Structure: Austenite with delta ferrite. This fluxcored wire offers higher productivity, higher …
- … of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing layers should be …
- … deposit is capable of taking a high polish.Structure: Austenite with delta ferrite UNS 34780 … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) / …
- … alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, 1.4002, 1.4016, 1.4057, …