1. … in case off multi-layer welding. The weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you …
  2. … one of “The first seamless rutile FCW with extreme low hydrogen for S690” Excellent for use in positional welding where high deposition … 1.8927, 1.8931, 1.8928, 1.8974,  1.7147, 1.7149, 1.8734 S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, 20MnCr65, 28CrMn4-3 L480 - L550, X65, … Q, 620 QL, 620 QL1, aldur 700 Q, 700 QL, 700 QL1, Salzgitter S700MC, Ympress Steel E690 TM, S700MC, Amstrong Ultra 650MC, 650 MCt, 700 MC….. … …
  3. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good …
  4. … of up to 550°C. Typical applications are in power plant construction, pressure pipe, turbine and boiler construction. The alloy is also used …
  5. … temperatures up to 600°C. The weld metal is resistant to high hydrogen pressure. … 12crmo19.5, GS-12crmo19.5, 1.7362, 1.7363     … E CrMo5 … A …
  6. … The weld puddle is amazingly fast freezing and therefore especially preferred in vertical down position with high speed and deep …
  7. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  8. … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  9. … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 …
  10. … alloys and covers a huge range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, …