1. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or …
  2. … The presence of tin improves the fluidity and is useful to increase the …
  3. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  4. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  5. … N/mm2 est déjà extrêmement difficile et les restrictions T-8/5 sont presque impossibles à respecter dans la pratique. Habituellement, des …
  6. … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO …
  7. … a copper coated welding wire for welding of high strength steels, used predominantly after stress relieving. May find its use for joining …
  8. … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and …
  9. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625P …
  10. … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected …