1. … Absolutely crack resistant  weld metal conditioned by the high-basic slag in combination with very low …
  2. … non-oxidizing liquids and are recommend for internal and external diameters. Using the combustion wire spray process, CEWELD® SP 1.4302 …
  3. … has better elevated temperature properties than Grade 2 or 3 and is sometimes specified for pressure vessels or piping for its superior …
  4. … Filler metal specifically intended for high integrity structural service at …
  5. … Weld metal deposited by SA Nicro 600 has high strength and good corrosion …
  6. … production process the hydrogen content is below 3ml/100g weld metal even after long storage in unconditioned condition. … Type …
  7. … Latest generation basic slag guarantees optimum metallurgical quality and attractive welder appeal. The weld deposit …
  8. … and reheat cracking. NILO Alloy 36 is available for Tig, Mig and SAW process. … NILO Alloy 36, Invar, cast Iron … NILO Alloy 36 …
  9. … of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where …
  10. … resistance over an ER409 alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, …