- … easy slag removal. Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production …
- … stability and easy slag removal with low spatter losses. Developed for high impact strength properties at extreme sub zero temperatures. …
- … Solid welding wire of the 12% Cr, 4.5% Ni, 0.5% Mo type. … 1.4317, 1.4313, …
- … grades 321 and 347. But also for unstabilized alloys like 304 or 304L. High resistance against intergranular corrosion. Fused flux FL 880 of …
- … High wear resistance and austenitic structure deposits. The deposit …
- … Corrosion resistance is higher than 5Cr-0.5Mo steels requirements. To be used with shielding …
- … excellent ductility due to Mn content Excellent corrosion resistance. Welding instructions: Start the electrode with about 130% hot start and …
- … against thermal shock, abrasion, erosion, corrosion and cavitation at high temperature and excellent resistance to many forms of mechanical …
- … Due to the high resistance to cracking and toughness, all weld metal requires no …
- … Abrasion combined with higher temperatures. … Hotworking tools, high speed tool steels, HSS, aluminium press molts, dies, stamping …