1. Austenitic deposit with strain hardening properties and no limits in …
  2. … offers a easily machinable weld deposit with high ductility and no undercut. … Welding ductile, grey and malleable cast irons. CEWELD® …
  3. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
  4. … Excelent weldabillity with fully austenitic weld metal with high resistance against stress corrosion …
  5. … alter the surface electrochemistry of the material in the crevice or under a surface deposit. Grade 12 has better elevated temperature …
  6. Austenitic filler metal for stabilized and non-stabilized CrNi steels. … down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1  Austenit ≤ 19 % Cr 9%Ni ,TÜV 1000: Gr. 21 - 22 (29 max.350°C), …
  7. … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …
  8. … layer in case off multi-layer welding. The weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in …
  9. … all weld metal requires no buffer layer except on materials considered critical or in case of old hardsurfacing layers. The weld deposit …
  10. … all weld metal requires no buffer layer except on materials considered critical. In this situation CEWELD AA M690 is recommended. Suited …