1. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  2. … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected …
  3. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  4. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or …
  5. … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO …
  6. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625P …
  7. … Alloy 740H is a nickel-base, precipitation hardenable superalloy that offers a unique combination of …
  8. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Stone …
  9. … a copper coated welding wire for welding of high strength steels, used predominantly after stress relieving. May find its use for joining …
  10. … and down hand welding. Excellent against pitting and stress corrosion.PREN above 35 weldmetal offers outstanding resistance against pitting. …