1. … to use only one wire to cover more procedures up to 550 MPa yield strength steels. It can also be used for constructions that needs post …
  2. … Excelent corrosion resistance combined with high strength due to the addition of copper. The filler metal shows remarkable …
  3. … -techniken entwickeln sich ständig weiter. Obwohl alle zumutbaren Anstrengungen unternommen wurden, um die Richtigkeit der enthaltenen …
  4. … deposit of less hardness. Overlays on steel with high tensile strength have to be buffered with CroNi 29/9 HL or 4370 HL. Equivalent in …
  5. … slag removal with low spatter losses. Developed for high impact strength properties at extreme sub zero temperatures. Hydrogen content is …
  6. … Excellent weldabillity and good mechanical strength combined with good corrosion resistance against seawater are …
  7. … Weld metal provides optimum strength and oxidation resistance above 815 °C (1500°F) up to 1149 °C …
  8. … The weld deposit will show release cracks to offer better bonding strenght with the base metal. More than 1 layer should not be deposited. A …
  9. … temperature so the minor alloy additions responsible for its creep strength are kept above the minimum considered necessary to ensure …
  10. … be achieved with extreme hardness of 800-1300 HV0.3 and adhesion strength of more than 70 MPa. In comparison to WC-Co, coatings from CEWELD …