1. … layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old layers. Weldable without protective gas.  … HRc …
  2. … This Nickel weld deposit offers a easily machinable weld deposit with high …
  3. … acids. The weld metal is corrosion resistant in sea water. The nickel content of this alloy makes it resistant to chloride-ion …
  4. … pitting and stress corrosion cracking due to its high chromium and nickel contents. … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV 1000: Gr. …
  5. … 760 and 870°C) for 16,000 hours. Suitable for joining and cladding Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. …
  6. … layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old layers. Weldable without protective gas. … Cement …
  7. … Titanium carbides. The choice for the buffer layer is depending on the base metal and not always necessary.  … HRc 54-59, hardfacing alloy for …
  8. … Rutile Fe, Cr, Co and Mo based elektotrode with high hot wear resistance, tensile strenght and a …
  9. …  wire  is  used  for  welding  matching,  and  similar, composition  base  materials.  The  weld deposit from Typ 15CrMoV6 provides  high …
  10. … < 1,2% C ( Kohlenstoff). Weitere Legierungsbestandteile, insbesondere Nickel, Molybdän, Titan und Niob, verbessern die …