1. … spatter loss, easy slag removal. Suitable for economic welding of Mo-steels up to 500°C. … Typ 0,5Mo  ≤ 460 MPa,  ISO 15608: 1.2, 1.3 …
  2. … with a remarkable low hydrogen content.  The requirements of the steels mentioned are obtained in normalized (N) and in air quenched (A) … in the stress relieved condition. … Base metal DIN EN ASTM Fine grain steel N+A - WStE 315 till 420 StE 315 till StE 420 EStE 315 till EStE …
  3. … Root is a thick basic-rutile coated electrode for welding low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root …
  4. … solutions (a form of degradation to which the austenitic stainless steels are prone).It is able to withstand a wide range of oxidizing and …
  5. … for dissimilar welds in Superaustenitic and Superduplex stainless steels or combinations of these with nickel base alloys. Some … this situation. … duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C4, …
  6. … and crevice corrosion, dissimilar joint of nickel alloys and stainless steels, … NiCrMo-4 2.4819, 1.7752, 2 NiMo16Cr15W ASTM B574, SB574, …
  7. … to -60 °C. Applications include structural, oil and gas and offshore steelwork. … Reh ≤ 960 MPa ISO 15608: ~3.1, 3.2 (Reh > 690 MPa) 1.8796, …
  8. … Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production process the …
  9. … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. CEWELD 4842 Ti has good general …
  10. … SA Alloy 825 strip is developed for cladding lower alloyed or steel parts to obtain protection against the earlier mentioned attacks …